Group: Forum Members
Posts: 2.5K,
Visits: 28K
|
With regards to the effect of carbon fibre on IAT, I've logged over 50 hours of dyno time testing specifically that - I can confirm that the difference is absolutely negligible, and if anything carbon fibre is slightly better than metal. There's a lot more influencing that than simply the thermal conductivity of the intake pipe material, so that small variable has very very little effect.
|