Group: Forum Members
Posts: 2.5K,
Visits: 28K
|
The tooling pre-pregs are very resin rich, so they are much tackier and harder to work with than the component pre-pregs. I remember having the same struggles, it is normal. You just have to try to get between the resin and the film, dont try to pull the film off if you havent got under the resin.
On some pieces I did find it easier to leave them over sized initially, then cut them down a bit once the film was removed. That way I could cut off the outer bits where the resin had come away.
|