I accidentally dripped some glass Cast 3 on a Matt tiled floor. I was thinking of sanding it down and then using a solvent. Different places online suggest paint stripper or acetone. 

Any suggestions please?
Warren (Staff)
Warren (Staff)
Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
As it is relatively fresh, acetone might help.  Otherwise try and chip it off from the side, you might be ok if there are traces or grease or some cleaning products which might mean it doesn't stick so well.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search