By rachelreveley - 4/24/2018 10:11:21 AM

I accidentally dripped some glass Cast 3 on a Matt tiled floor. I was thinking of sanding it down and then using a solvent. Different places online suggest paint stripper or acetone. 

Any suggestions please?
By Warren (Staff) - 4/24/2018 12:05:14 PM

As it is relatively fresh, acetone might help.  Otherwise try and chip it off from the side, you might be ok if there are traces or grease or some cleaning products which might mean it doesn't stick so well.