Author
Message
Robi_redman
R
Forum Member (27 reputation)Forum Member (27 reputation)Forum Member (27 reputation)Forum Member (27 reputation)Forum Member (27 reputation)Forum Member (27 reputation)Forum Member (27 reputation)Forum Member (27 reputation)Forum Member (27 reputation)
Group: Forum Members
Posts: 4, Visits: 20
Hi new to the carbon skinning done a few parts in the past but only small items. Iv have just done a larger part and all went well until fitted back to the car. It looks and feels as if the resin has sunk and gone all waveie and not smooth to touch although the resin is still solid. They were also 2k clear coated after words aswell. And was plenty of coats applied so is built up nicely

I also did some mirror caps at the same time and they are still perfect and not gone like the other part at all.

The parts are fitted to the external of the car so I thought it may be to do with the heat of the weather but looking at the temp it should withstand it should be fine

If any one could shed some light on why it’s doing this that would be great as I’m baffled lol.

I have added a couple of pictures but it doesunt really show up as bad


Reply
Robi_redman
R
Forum Member (27 reputation)Forum Member (27 reputation)Forum Member (27 reputation)Forum Member (27 reputation)Forum Member (27 reputation)Forum Member (27 reputation)Forum Member (27 reputation)Forum Member (27 reputation)Forum Member (27 reputation)
Group: Forum Members
Posts: 4, Visits: 20
Thanks for the reply. What would you recommend I do now take it back off sand it back down and re resin it How long do I need to leave it for the post cure.

Thanks Robbie