A strip of rigid polypropylene would work well. You could hot melt glue it in place, then seal any gaps with silicone sealant. if its a bit too floppy then use a wooden batten behind it to hold it in place.
Once the resin has cured, the polypropylene will easily peel off the edge as epoxy does not stick to polypropylene.