Can also just use a piece of wood covered with flashbreaker tape. Bit riskier than polypropylene, as any resin bleed under the tape and into the wood will bond the wood to your floor, so you need to be sure the tape is stuck down well. But with a clean piece of wood this is quite easy.
My personal preference would still be Warren's suggested method, but in case you were looking for a simpler/cheaper method.
|