Hello,

I´m with difficulty to make total vaccum.

I´ve tried 3 times, with 3 diferent moulds, and never achieved total vaccum, there´s always a leak.

I´ve checked the gum tape several times, and nothing.

So i´ve tried with a Trough Bag connector at the vaccum line, and  the feed line without connector, only the pvc hose with gum tape.

The result was the same, so i decided to make some tests.

First test:

With the Trough bag connector closed, i´ve switched on the pump, and when the gauge indicator got to the end, i´ve closed the pump valve, and then switched off. The gauge indicator moved, so there is a leak somewhere between the Trough bag connector and the pump.

There´s a few fotos taken with 2 minutes between them:

http://i675.photobucket.com/albums/vv112/pedcrist/P8060081.jpg

http://i675.photobucket.com/albums/vv112/pedcrist/P8060083.jpg

http://i675.photobucket.com/albums/vv112/pedcrist/P8060085.jpg

http://i675.photobucket.com/albums/vv112/pedcrist/P8060086.jpg

http://i675.photobucket.com/albums/vv112/pedcrist/P8060088.jpg

http://i675.photobucket.com/albums/vv112/pedcrist/P8060089.jpg

http://i675.photobucket.com/albums/vv112/pedcrist/P8060091.jpg

Second test:

With the Trough bag connector closed, i´ve switched on the pump, and when the gauge indicator got to the end, i´ve clamped the vac hose between the Trough bag connector and the catch pot, closed the pump valve, and then switched off. The gauge indicator moved not so fast as the first test, but moved, so there still´s  a leak.

There´s a few fotos taken with 2 minutes between them:

http://i675.photobucket.com/albums/vv112/pedcrist/P8060092.jpg

http://i675.photobucket.com/albums/vv112/pedcrist/P8060093.jpg

http://i675.photobucket.com/albums/vv112/pedcrist/P8060094.jpg

http://i675.photobucket.com/albums/vv112/pedcrist/P8060095.jpg

http://i675.photobucket.com/albums/vv112/pedcrist/P8060096.jpg

http://i675.photobucket.com/albums/vv112/pedcrist/P8060097.jpg

I don´t know what´s happening, if someone know, please give me a help.

Another issue: When i connect the vac hose to the silicone connector, i´ve got to cut it to be more thin, otherwise the tube won´t fit in the hole with the bag thickness.

Thanks,

Pedro
Reply
baja_patient
baja_patient
Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)
Group: Forum Members
Posts: 135, Visits: 1.6K
I have a suspicion what this could be. (Also a note to Easycomposites!!)

The connector on the catchpot, the black cable throughpass clamp where the resin line enters the catchpot, that fitting is installed with a piece of cut off silicone hose, at least on mine it was.

It is not the correct seal for the application and it does in deed not seal.

I went to my o-ring kit and chose the appropriate size, can measure it for u if you dont have a kit (very affordable and useful in the house) i put the o-ring on there and gave it a very slight tightening with a wrench. Only light cos its made of plastic. Seals perfectly. That pump valve should be fine. Try the connector!

cheers
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
pedcrist - 13 Years Ago
Kevin-Lee - 13 Years Ago
Warren - 13 Years Ago
pedcrist - 13 Years Ago
SebRS - 13 Years Ago
Kevin-Lee - 13 Years Ago
Warren - 13 Years Ago
pedcrist - 13 Years Ago
baja_patient - 13 Years Ago
pedcrist - 13 Years Ago
neilb - 13 Years Ago
fgayford - 13 Years Ago
baja_patient - 13 Years Ago
fgayford - 13 Years Ago
fgayford - 13 Years Ago
                     thanks for sharing that information!
matthieutje65 - 13 Years Ago
prairiecustomcomposites - 13 Years Ago
fgayford - 13 Years Ago
Daz - 13 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search