Hi.
I have I 3D printed rc plane (120cm wingspan) that I thinking about to cover with woven glass fabric for strength och looks. Thinking about this 
https://www.easycomposites.co.uk/glass-cloth/light-weight-100g-woven-glass-fabric.html 

Do I need do something with the surface of plane before hand laying the fiber glass or any other tips I will be thankfull? The plane will be printed in PLA.


Thanks.

/F









Edited 7 Years Ago by Felat B
scottracing
scottracing
Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)
Group: Forum Members
Posts: 460, Visits: 5.2K
Ive recently done some skinning of PLA printed parts, epoxy sticks really well to PLA and all i done was sanded with 240grit paper and cleaned up with acetone.

You can either use shrink tape once you have wetted out the material to give you a better surface finish and less sanding, but the XCR skinnign resin and the material you have chosen should work well.