Group: Forum Members
Posts: 460,
Visits: 5.2K
|
Ive recently done some skinning of PLA printed parts, epoxy sticks really well to PLA and all i done was sanded with 240grit paper and cleaned up with acetone.
You can either use shrink tape once you have wetted out the material to give you a better surface finish and less sanding, but the XCR skinnign resin and the material you have chosen should work well.
|