Group: Forum Members
Posts: 53,
Visits: 478
|
I am no expert at all but I have been reading around some to learn for my own projects.. When the part is fully infused you clamp the vacuum port first. Then you let the epoxy flow some more before you close the epoxy feed valve. 10-30 sec or so Also you might benefit from a epoxy "flow brake" around the vacuum port.. A glitch in the flow mesh. Size of it depends..
Exactly how to do these things depends of the size of the part and a bunch of other stuff so i cant help you much moore.
|