shelf life relase agent and wax additive solution MW


Author
Message
Adelbolide
Adelbolide
Supreme Being (187 reputation)Supreme Being (187 reputation)Supreme Being (187 reputation)Supreme Being (187 reputation)Supreme Being (187 reputation)Supreme Being (187 reputation)Supreme Being (187 reputation)Supreme Being (187 reputation)Supreme Being (187 reputation)
Group: Forum Members
Posts: 16, Visits: 112
Hello,
is there a shelf life for release agents and wax additive solution MW. I'm having some problems with this products. Recently I used a release agent I've opened some time ago (1 year) and it didn't work very well.

I've also a wax additive I bought 6 months ago. I opened it only now and the product became solid.

Is there a shelf life for this products? A best use date after opening?

Thanks in advance
Reply
Warren (Staff)
Warren (Staff)
Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Sounds like maybe the lid was loose?


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search