By Adelbolide - 3/25/2018 9:23:21 PM
Hello, is there a shelf life for release agents and wax additive solution MW. I'm having some problems with this products. Recently I used a release agent I've opened some time ago (1 year) and it didn't work very well.
I've also a wax additive I bought 6 months ago. I opened it only now and the product became solid.
Is there a shelf life for this products? A best use date after opening?
Thanks in advance
|
By Warren (Staff) - 3/27/2018 8:24:06 AM
Sounds like maybe the lid was loose?
|
|