 You actually have quite a bit of choice. We do a range of Epoxy compatible pigments for solid opaque colours as well as 10 different tinting pigments.  However there is a wider range out there in the art and craft side of the market including more colours, metal flakes etc.  Most of them will be fine with epoxy, however it is always worth asking the question of the pigment manufacturer and if you are really unsure then its worth doing a small test piece to see how it comes out.
 
 
 Warren Penalver
 Easy Composites / Carbon Mods - Technical Support Assistant
 
 |