Epoxy repelling on mould


Author
Message
AWOL
A
Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)
Group: Forum Members
Posts: 9, Visits: 72
Hey Guys,

We're playing around with a few moulds at home (Australia) but are having a consistent repelling issue from the Epoxy when we go to lay our carbon (240gsm 2/2 twill)
Pretty much pulling our hair out, we're convinced it may have something to do with our moulds but thought we'd seek opinion from the global community.
We're wondering if it is because of a polyester gelcoat mould vs epoxy problem? 
Anyway - here's what we have;

Mould build - the moulds always seem to be a good representation and quite solid
Release waxed mould - 5 times
Laid down polyester gelcoat (waited 24hours)
Laid down 1st lightweight fibreglass adhesion coat (waited 24hours)
Laid down 5-6 heavyweight fibreglass layers
Wait 2 days - pull mould - reverse mould looks great, detailed representation

Laying Carbon - temperature is approx 20-25C
Waxed mould - 5 times, waiting between coats
PVA release agent - light coat - wait 30 mins til applying epoxy 
Epoxy is West Systems with 205 hardener 5:1
Yet when we go to brush on epoxy it repels, ie doesn't seem to want to stick to the prepped surface

Note: when we skin items we have no issues with the epoxy

We're still noobs in this hobby, so will appreciate any input

kind regards
Justin

Replies
AWOL
A
Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)
Group: Forum Members
Posts: 9, Visits: 72
Here's a pic - probably should mention we're doing hand layup, and its 480gsm 2/2 twill
The areas where it has repelled the epoxy show up as great gaping voids Ermm



Hoping to resurrect it - or even lay up a new attempt, because it's going to look cool - for a mate's 70 Mach 1 

Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
AWOL - 2/28/2018 12:07:39 AM
Here's a pic - probably should mention we're doing hand layup, and its 480gsm 2/2 twill
The areas where it has repelled the epoxy show up as great gaping voids Ermm



Hoping to resurrect it - or even lay up a new attempt, because it's going to look cool - for a mate's 70 Mach 1 

Did you try using a plastic roller to remove air/spread excess resin. 
I see you add multiple layers of carbonfiber. I assume you wet the mould with epoxy, put down the first layer of carbonfiber, wet it out, add new layer of carbon fiber, wet it out again? 
  


Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




AWOL
A
Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)
Group: Forum Members
Posts: 9, Visits: 72
matthieutje65 - 3/1/2018 8:56:58 AM

Did you try using a plastic roller to remove air/spread excess resin. 
I see you add multiple layers of carbonfiber. I assume you wet the mould with epoxy, put down the first layer of carbonfiber, wet it out, add new layer of carbon fiber, wet it out again? 
  

Thanks for the reply Matthieu,
No we haven't tried a plastic roller yet, we will source one out for sure, especially if it will improve our chances - I'm not going to pretend we are experts, still learning (perhaps too impatient)
Yes, we did attempt to wet out the mould first with epoxy, (it seemed to repel away - like water on wax, literally runs away from the surface .. unless our wax buffing needs work 'OP quietly questions his wax & PVA methods')
We then lay the first layer of cloth, we hoped we could wet it out enough to wet right through to counteract the repelling resin, and actually looked to cover quite well 
We let this tack off a bit then laid some more cloth, wetting it out also

Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
AWOL - 3/1/2018 9:18:02 AM
matthieutje65 - 3/1/2018 8:56:58 AM

Did you try using a plastic roller to remove air/spread excess resin. 
I see you add multiple layers of carbonfiber. I assume you wet the mould with epoxy, put down the first layer of carbonfiber, wet it out, add new layer of carbon fiber, wet it out again? 
  

Thanks for the reply Matthieu,
No we haven't tried a plastic roller yet, we will source one out for sure, especially if it will improve our chances - I'm not going to pretend we are experts, still learning (perhaps too impatient)
Yes, we did attempt to wet out the mould first with epoxy, (it seemed to repel away - like water on wax, literally runs away from the surface .. unless our wax buffing needs work 'OP quietly questions his wax & PVA methods')
We then lay the first layer of cloth, we hoped we could wet it out enough to wet right through to counteract the repelling resin, and actually looked to cover quite well 
We let this tack off a bit then laid some more cloth, wetting it out also

hmm strange! I would recommend you to try the same technique you are using on a glass plate! that way you can do every step and try to analyze now and then through te glass wat is happening on the surface. That way you will already be able to see if the carbonfiber is wetting out enough and if the resin is working ok to go through the fibers till mould surface 


Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




AWOL
A
Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)
Group: Forum Members
Posts: 9, Visits: 72
Matthieu Libeert - 3/1/2018 9:32:52 AM

hmm strange! I would recommend you to try the same technique you are using on a glass plate! that way you can do every step and try to analyze now and then through te glass wat is happening on the surface. That way you will already be able to see if the carbonfiber is wetting out enough and if the resin is working ok to go through the fibers till mould surface 

That's a great idea - I'll try that for sure (on a smaller scale haha)
Thanks again for the advice .. stay tuned 

Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
AWOL - 3/1/2018 10:11:45 PM
Matthieu Libeert - 3/1/2018 9:32:52 AM

hmm strange! I would recommend you to try the same technique you are using on a glass plate! that way you can do every step and try to analyze now and then through te glass wat is happening on the surface. That way you will already be able to see if the carbonfiber is wetting out enough and if the resin is working ok to go through the fibers till mould surface 

That's a great idea - I'll try that for sure (on a smaller scale haha)
Thanks again for the advice .. stay tuned 

No problem, hopes everything turns out ok for you! 


Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
AWOL - 8 Years Ago
AWOL - 8 Years Ago
AWOL - 8 Years Ago
matthieutje65 - 8 Years Ago
AWOL - 8 Years Ago
matthieutje65 - 8 Years Ago
AWOL - 8 Years Ago
                             No problem, hopes everything turns out ok for you!
matthieutje65 - 8 Years Ago
Dravis - 8 Years Ago
AWOL - 8 Years Ago
M.R. - 8 Years Ago
AWOL - 8 Years Ago
Hanaldo - 8 Years Ago
AWOL - 8 Years Ago
CaveDweller - 8 Years Ago
CaveDweller - 8 Years Ago
AWOL - 8 Years Ago