HI how would i go about covering a VW MK1 Dashboard with Carbon Fibre
Reply
Matt (Staff)
Matt (Staff)
Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
Hi Marlonji,

It looks good to go. Early VW dashes are a very angular affair and so I think I would be considering doing the large flat sections in one peice and the 'inside' edges of the binnacle as a separate strip.

In reality on this job I think the angular shape of it will work in your favour. I would suggest using ProFinish cloth which is like a normal 2/2/ twill but it has a binder on the back which holds the cloth stiffer stopping the weave from distorting and also allowing you to put very neat join/join lines in it. ProFinsih will also allow you to to make separate strips for the inside of the binacle and some of the other 'sections' that would otherwise require too much weave distortion.

--Matt

Matt Statham
Easy Composites / Carbon Mods - Technical Sales
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search