	Group: AdministratorsPosts: 2.5K, 
    Visits: 8.5K
 
 | 
                    
			            GlassCast 3 has no problems with underfloor heating.  In fact, this time of year, if it is working, switch it on during the curing process and it will help speed up the cure. 
 With an uneven slab, you will need to take into account how uneven it is in your resin calculations.  You may need more resin than a perfectly flat floor so that you don't end up with one end of the room  with no resin after it has self leveled.
 
 GlassCast  will to an extent be slippery when wet - all gloss surfaces will be.  However in our and our customers experience, it is no more slippery than the commonly used gloss ceramic tiles found in many bathrooms and kitchens these days.
 
 
 Warren Penalver
 Easy Composites / Carbon Mods - Technical Support Assistant
 
 |