By Helgatron - 2/26/2018 11:04:08 AM
I'm thinking of doing a version of the penny floor in a small bathroom area, using washers rather than pennies. The existing floor is poured concrete with underfloor heating. The concrete is quite rough and ready and a bit uneven. There'll be a shower cubicle, so every chance of the floor getting wet. So, can i use Glasscast over an underfloor heated concrete floor and will the finished surface be too slippery for a bathroom floor?
Many thanks
|
By Warren (Staff) - 3/5/2018 10:36:43 AM
It is not something we have tried before but I don't see why it wouldn't work as long as the floor is fully dry. You could do 2 pours to help with the pinhole issue or skim a very thin layer over the surface to fill in the pinholes then go with a main pour afterwards.
|
|