andy47 - 2/17/2018 5:05:01 PM
I want to reinforce an existing semi-flexible part with carbon fiber and a core material to make it as rigid as possible. I would lay up a few layers of carbon fiber over the surface, then a core material and then more layers of carbon fiber. In order to achieve a good adhesion between the layers and especially the core material, I would put the part in a vacuum bag. Is it a good idea? Can I use Lantor Soric (2mm) as a core material? I see Lantor Soric is designed for resin infusion, but it seems epoxy can flow through it, but I am not sure.



Soric is great for infusion, but I would be afraid of leaving large voids in a hand layup.  I would just use a foam designed to be used as a core.  If you are going to vacuum bag the part anyway, the little extra effort to infuse it is well worth it. 

Edited 8 Years Ago by polaraligned
andy47
a
Supreme Being (162 reputation)Supreme Being (162 reputation)Supreme Being (162 reputation)Supreme Being (162 reputation)Supreme Being (162 reputation)Supreme Being (162 reputation)Supreme Being (162 reputation)Supreme Being (162 reputation)Supreme Being (162 reputation)
Group: Forum Members
Posts: 22, Visits: 95
I want to reinforce an existing semi-flexible part with carbon fiber and a core material to make it as rigid as possible. I would lay up a few layers of carbon fiber over the surface, then a core material and then more layers of carbon fiber. In order to achieve a good adhesion between the layers and especially the core material, I would put the part in a vacuum bag. Is it a good idea? Can I use Lantor Soric (2mm) as a core material? I see Lantor Soric is designed for resin infusion, but it seems epoxy can flow through it, but I am not sure.