Hi guys!

I am building spearguns for a 5-6 years. Most of them were wrapped with carbon cloth. Last two years I am using vacuum bagging for better results. I used to put one layer of epoxy resin and wait for 2-3  hours and then put carbon cloth. Recently I decide to use this spray adhesive for reducing waiting. Gun was prepared, sanded and coated with one layer of epoxy resin.  Sanded again with grit 100-10 and sprayed with adhesive. After 2-3 minutes I put on carbon cloth and proceed with resin, peel ply, breather cloth, vacuum bag and pump was turned on for several hours. I was satisfied how everything goes on.
Tommorom I remove speargun from bag. Looked great; but when cutting off exceed carbon cloth I noticed that it was not hard glued to guns body. On a first sight it was perfect but I was able to remove it like a socks.
Can anyone tell me what I was doing wrong?

Thx

 
ChrisP
ChrisP
Supreme Being (75 reputation)Supreme Being (75 reputation)Supreme Being (75 reputation)Supreme Being (75 reputation)Supreme Being (75 reputation)Supreme Being (75 reputation)Supreme Being (75 reputation)Supreme Being (75 reputation)Supreme Being (75 reputation)
Group: Forum Members
Posts: 9, Visits: 281
I think from what you are saying, that you are using FusionFix for the wrong purpose. It is designed as an in-mould temporary adhesive not a permanent adhesive for bonding of carbon (or any material)
Chris
neno2812
neno2812
Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)
Group: Forum Members
Posts: 3, Visits: 13
ChrisP - 1/25/2018 3:37:26 PM
I think from what you are saying, that you are using FusionFix for the wrong purpose. It is designed as an in-mould temporary adhesive not a permanent adhesive for bonding of carbon (or any material)
Chris



neno2812
neno2812
Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)
Group: Forum Members
Posts: 3, Visits: 13
ChrisP - 1/25/2018 3:37:26 PM
I think from what you are saying, that you are using FusionFix for the wrong purpose. It is designed as an in-mould temporary adhesive not a permanent adhesive for bonding of carbon (or any material)
Chris


Thx for fast answer!
 I'll use it for that purpouse. I was hoping it could spare me a lot of time.
Warren (Staff)
Warren (Staff)
Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
As said, it's not really it's design purpose.  That being said, epoxy will cross link across fusion fix when used sparingly.  It means it can be used in the middle of a laminate stack without it causing any structural issues.

However it is all about using it lightly.  The smallest of dusting should be all you need, in which case the resin should still be able to soak through the cloth to surface to get a good bond.

From the pictures, the wood does look too smooth with a bit of shine to it.  The surface should have a nice coarse key to it for maximum adhesion.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search