Hi, 
I'm an Italian student who start using your products for the rinforce of a quarter scale model of a vault built with timber block, then tested to shear displacements  at the springings. Now I have to import my model on Abaqus and I need the mechanical properties of this reinforce. In particoular I've used: 
-    Lightweight flat braid 
-    Epoxy hardener
-    EL2 Laminating epoxy
-    Fumed silica
 Where can I find Young modulus, or yield stress of the flat braid ? 
Thanks in advance 
Warren (Staff)
Warren (Staff)
Supreme Being (36K reputation)Supreme Being (36K reputation)Supreme Being (36K reputation)Supreme Being (36K reputation)Supreme Being (36K reputation)Supreme Being (36K reputation)Supreme Being (36K reputation)Supreme Being (36K reputation)Supreme Being (36K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Welcome to the forum.  The datasheets for those products are available on the product pages for you to download.  There is no mechanical data as such for the fumed silica as it is used as a thickener for resin systems.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Reading This Topic

Explore
Messages
Mentions
Search