By Luciaz - 1/25/2018 12:07:50 PM
Hi, I'm an Italian student who start using your products for the rinforce of a quarter scale model of a vault built with timber block, then tested to shear displacements at the springings. Now I have to import my model on Abaqus and I need the mechanical properties of this reinforce. In particoular I've used: - Lightweight flat braid - Epoxy hardener - EL2 Laminating epoxy - Fumed silica Where can I find Young modulus, or yield stress of the flat braid ? Thanks in advance
|
By Warren (Staff) - 1/25/2018 1:10:25 PM
Welcome to the forum. The datasheets for those products are available on the product pages for you to download. There is no mechanical data as such for the fumed silica as it is used as a thickener for resin systems.
|
|