Second layer (coat) on GlassCast epoxy resin on tiled floor


Author
Message
kubla
k
Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)
Group: Forum Members
Posts: 2, Visits: 5
Hi, is it possible to lay a second layer of resin onto a fully cured floor (3-5mm). There are small areas where the resin is a bit thin and wondered if it's possible re-coat these areas with small amount of resin to thicken it up a bit. Or is it a case of having to pour another whole area over the whole floor?....it's about 1.5 metres square? Thanks





Replies
Kimberley1985
K
Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)
Group: Forum Members
Posts: 3, Visits: 10
Hello Smile

I’m not sure how to write a question of my own, so apologies for jumping in here!
I have done a penny table and have used epoxy resin and hardener on top, however in some places it is very tacky, and some places also look wet underneath the cured resin. what do you advise I do to rectify this? Also can I re resin just the areas in question or would I need to re resin the whole lot again? Any help would be greatly appreciated, thank you so much
Kim x
Interloper393
Interloper393
Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)
Group: Forum Members
Posts: 90, Visits: 634
Kimberley1985 - 1/24/2018 11:59:20 PM
Hello Smile I’m not sure how to write a question of my own, so apologies for jumping in here! I have done a penny table and have used epoxy resin and hardener on top, however in some places it is very tacky, and some places also look wet underneath the cured resin. what do you advise I do to rectify this? Also can I re resin just the areas in question or would I need to re resin the whole lot again? Any help would be greatly appreciated, thank you so much Kim x

Of your using epoxy then I don' think it was mixed well enough of its still tacky and soft

Kimberley1985
K
Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)
Group: Forum Members
Posts: 3, Visits: 10
That was what I thought. Is there anything that can be done or should I scrap it?
Thanks for replying!
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
kubla - 9 Years Ago
Warren (Staff) - 9 Years Ago
kubla - 9 Years Ago
Kimberley1985 - 8 Years Ago
Interloper393 - 8 Years Ago
Kimberley1985 - 8 Years Ago
Hanaldo - 8 Years Ago
Kimberley1985 - 8 Years Ago
Warren (Staff) - 8 Years Ago
oekmont - 8 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search