Treated Carbon or Graphite fibres.


Author
Message
Umesh Marathe
Umesh Marathe
Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)
Group: Forum Members
Posts: 2, Visits: 3
Does easy composites supply treated carbon or graphite fibres/fabric?

Reply
Umesh Marathe
Umesh Marathe
Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)
Group: Forum Members
Posts: 2, Visits: 3
Warren (Staff) - 1/12/2018 4:53:32 PM
What kind of treated fibres do you mean? Some fabrics have special coatings for certain applications and almost all carbon fibre will have a sizing added to the fibre during manufacture.

I mean surface treatment like oxygen nitrogen plasma, etching by HNO3 acid on bare carbon fibres. We need such kind of treated fibres.