+x oekmont - 1/9/2018 9:00:26 AMI've had similar effects caused by moisture. the storage of the resin might be too cold, so that water condense on the resin, once it's in the mixing pot.Do you degas your resin before the process? This can be a countermeasure against moisture. Additionally the degassing foam wich occurs without pre-degassing might cumulate in bridging areas, and produces this opaque resin after the compression. Do you have the access to a microscope for a mircosection?