Rigidity and flexibility of CF Tubes


Author
Message
Job_CF
J
Forum Guru (58 reputation)Forum Guru (58 reputation)Forum Guru (58 reputation)Forum Guru (58 reputation)Forum Guru (58 reputation)Forum Guru (58 reputation)Forum Guru (58 reputation)Forum Guru (58 reputation)Forum Guru (58 reputation)
Group: Forum Members
Posts: 6, Visits: 26
Hi
I am looking to build a trike unit for a microlight aircraft as in the photo.
but using CF tubes in place of the aluminium tubes.
Some tubes needs to be rigid with good tensile and compressive strength but with little or no flexibility.
The pair of undercarriage legs, 1 meter each, need to flex about 3 to 4 inches when landing.
Total weight including pilot is 170 kg.
Recommendations please on the type of CF tubes by Easy Composites.
Also is there a website or calculator to figure out how much a particular type of tube will flex for a given load?
Thanks!


Edited 8 Years Ago by Job_CF
Replies
oekmont
oekmont
Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)
Group: Forum Members
Posts: 550, Visits: 27K
f=(F*l^3)/(3*E*I)
f= deflection
l= length between support and wheel
E= Young's modulus
I= Moment of inertia

E depends on the laminate

Job_CF
J
Forum Guru (58 reputation)Forum Guru (58 reputation)Forum Guru (58 reputation)Forum Guru (58 reputation)Forum Guru (58 reputation)Forum Guru (58 reputation)Forum Guru (58 reputation)Forum Guru (58 reputation)Forum Guru (58 reputation)
Group: Forum Members
Posts: 6, Visits: 26
oekmont - 1/8/2018 2:16:19 PM
f=(F*l^3)/(3*E*I)
f= deflection
l= length between support and wheel
E= Young's modulus
I= Moment of inertia

E depends on the laminate
I know these two
MI for Solid Round Beams = (pi * (OD4 - ID4)) / 64
Deflection = (length^3 * force) / (3 * E * MI)
where
MI = Moment of Inertia
E = Modulas of Elasticity in psi

But two different Youngs Modulus figures given for this tube!
Youngs Modulus 0°(GPa)     90
Youngs Modulus 90°(GPa)   19
Which one to use?


GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Job_CF - 8 Years Ago
oekmont - 8 Years Ago
Warren (Staff) - 8 Years Ago
Job_CF - 8 Years Ago
Warren (Staff) - 8 Years Ago
oekmont - 8 Years Ago
Job_CF - 8 Years Ago
oekmont - 8 Years Ago
Job_CF - 8 Years Ago
oekmont - 8 Years Ago
Job_CF - 8 Years Ago
oekmont - 8 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search