I am looking to build a trike unit for a microlight aircraft as in the photo.
but using CF tubes in place of the aluminium tubes.
Some tubes needs to be rigid with good tensile and compressive strength but with little or no flexibility.
The pair of undercarriage legs, 1 meter each, need to flex about 3 to 4 inches when landing.
Total weight including pilot is 170 kg.
Recommendations please on the type of CF tubes by Easy Composites.
Also is there a website or calculator to figure out how much a particular type of tube will flex for a given load?
Thanks!


Edited 6 Years Ago by Job_CF
Reply
Warren (Staff)
Warren (Staff)
Supreme Being (15K reputation)Supreme Being (15K reputation)Supreme Being (15K reputation)Supreme Being (15K reputation)Supreme Being (15K reputation)Supreme Being (15K reputation)Supreme Being (15K reputation)Supreme Being (15K reputation)Supreme Being (15K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8K
The properties are similar based on our experience, due to similar construction (except for the surface finish).  However we do not have formal mechanical data for the woven finish tubes yet. 


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Job_CF - 6 Years Ago
oekmont - 6 Years Ago
Warren (Staff) - 6 Years Ago
Job_CF - 6 Years Ago
Warren (Staff) - 6 Years Ago
oekmont - 6 Years Ago
Job_CF - 6 Years Ago
oekmont - 6 Years Ago
Job_CF - 6 Years Ago
oekmont - 6 Years Ago
Job_CF - 6 Years Ago
oekmont - 6 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search