+x MarkMK - 12/21/2017 11:47:03 AMI use Cytec's Aerofix 3 with both 'bare' epoxy and in moulds with a polyester-based coating and it works great with both with little or no visible traces left behindIf that's available where you are I'd recommend trying that and a light mist is usually all that's necessary to hold things well, even on vertical surfaces