+x Tony2125 - 12/24/2017 7:53:19 AMNo, never triedThis seems to be a good solutionHowever do you know if it can ship to Europe ?I also struggle with custom made inflatable bladder so I would possibly be interested
+x Fasta - 11/22/2017 6:14:25 AMhttp://www.acmtucson.com/products/
+x Hanaldo - 12/4/2017 11:27:25 PM+x Worldtrvlr03 - 12/4/2017 10:29:23 PM+x FLD - 12/1/2017 7:35:31 PMWhy not use extruded polystyrene, cut it with a hotwire or sand as required. You can then use acetone to dissolve it out.Thanks that might work also.. You will want expanded polystyrene. Extruded is somewhat harder to dissolve.Horrifically messy and unhealthy process, I for one will never do it again.
+x Worldtrvlr03 - 12/4/2017 10:29:23 PM+x FLD - 12/1/2017 7:35:31 PMWhy not use extruded polystyrene, cut it with a hotwire or sand as required. You can then use acetone to dissolve it out.Thanks that might work also..
+x FLD - 12/1/2017 7:35:31 PMWhy not use extruded polystyrene, cut it with a hotwire or sand as required. You can then use acetone to dissolve it out.