Talk Composites - The Forum for Advanced Composites

Water soluble Foam core

http://www.talkcomposites.com/Topic24299.aspx

By Worldtrvlr03 - 11/22/2017 1:51:32 AM

I am looking for a water soluble foam core material I can you use, and then once the part is cured use water to wash it out. Preferably I do not want to use a CNC to machine it. Any suggestions are greatly appreciated. 
By Worldtrvlr03 - 12/26/2017 10:38:07 PM

Tony2125 - 12/24/2017 7:53:19 AM
No, never triedThis seems to be a good solutionHowever do you know if it can ship to Europe ?I also struggle with custom made inflatable bladder so I would possibly be interested

Thanks, I will look into it...