That is going to be far easier to make a 2 part item - an outer piece then inner moulding. To make it as a one piece part with split moulding would be extremely difficult IMO. You could make the mould but then the pull area would be a very thin area to try an lay up into - even as wet lay, let alone trying to get a bagging stack for more advanced processes.