By John Elshaw - 12/2/2017 9:10:55 PM
I've made some basic trim pieces and have had good success, now I want to try this door pull for my car. Where would you recommend I divide the mould sections? I'm guessing this will need to be 3 pieces, correct? Any help greatly appreciated.

|
By Warren (Staff) - 12/8/2017 9:08:13 AM
The screw block on the rear would almost certainly need to be bonded on separately, perhaps a piece of suitable plastic cut to shape or even make a mould and resin cast a block with a small flange around it to increase the bonding surface area and hence bond strength.
|
|