Handling spread tow cloth


Author
Message
FLD
FLD
Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)
Group: Forum Members
Posts: 468, Visits: 2.7K
I posted in the general section but figured its better here.

I've come across spread tow cloth in canoes and it looks awesome!  I fancy making a hard top for my car with it (purely because it looks good!!) but I'd obviously need to be careful with the weave pattern.  Has anyone got any experience with it in terms of how it drapes and how easy the weave is disturbed?  I've used 200g twill weave dry and found it moves if you're not careful.  I dont want to mess this up if I can help it.
Reply
Matt (Staff)
Matt (Staff)
Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
Hi FLD,

The spread-tow also needs to be handled with care in order to keep it in good alignment. Unless you're working with a completely flat surface (which the hard-top for your car will no be) then I would stear clear of the 25mm spread tow and, to be honest, probably the 15mm 2/2 twill weave spread tow. Both of these are too loose to work with on moulded/contoured surfaces if you're using them for cosmetic reasons rather than purely structural. The 15mm plain weave spread tow is more like a fabric you can use on a contoured surface - not a really complex one but some steady curves should be fine. The tows themselves are well bound together though and so you can individualy move them to ensure they're aligned as you want them to be, particularly whilst they're dry.

I hope this helps but if you're in any doubt, grab one of our reinforcement sample packs which include all of the spread-tow fabrics so you can have a feel of them before committing to the whole job.

I hope this helps,

All the best, Matt

Matt Statham
Easy Composites / Carbon Mods - Technical Sales
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search