I posted in the general section but figured its better here.
I've come across spread tow cloth in canoes and it looks awesome! I fancy making a hard top for my car with it (purely because it looks good!!) but I'd obviously need to be careful with the weave pattern. Has anyone got any experience with it in terms of how it drapes and how easy the weave is disturbed? I've used 200g twill weave dry and found it moves if you're not careful. I dont want to mess this up if I can help it.
|