Hello, im struggling to get my head around the mix ratio for the eproxy resin. On the containers, it says 100 - 30, is this measured by weight, or quantity? 

Let's say I wanted to use a small amount of resin for example 5 KG in weight? How do I work out how much harder to use? 

I have made a mixture and it's been drying for 24 hours, however its still tacky, im assuming I have not used enough hardner? 
Reply
oekmont
oekmont
Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)
Group: Forum Members
Posts: 550, Visits: 27K
[quote]
GreyArea - 11/30/2017 6:44:37 PM
Just a minor quibble. It’s great that you stick to parts by weight. But then you provide syringes for things like the MEKP hardener, which of course dispense by volume.
/quote]ex
Ec


Exactly. The important point here is "for mekp". Unlike epoxy "hardener" mekp is actually a hardener. The final structure of solid polyester is solely build of the resin component, mekp just starts the reaction. Therefore you can slightly change the mekp ratio, wich will affect the curing time. Anything between 1,5 and 2,5 % should be fine.

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
martynball - 8 Years Ago
oekmont - 8 Years Ago
Matt (Staff) - 8 Years Ago
Matt (Staff) - 8 Years Ago
martynball - 8 Years Ago
Matt (Staff) - 8 Years Ago
martynball - 8 Years Ago
GreyArea - 8 Years Ago
oekmont - 8 Years Ago
Warren (Staff) - 8 Years Ago
Capt Rouge - 8 Years Ago
Warren (Staff) - 8 Years Ago
Hanaldo - 8 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search