Hello, im struggling to get my head around the mix ratio for the eproxy resin. On the containers, it says 100 - 30, is this measured by weight, or quantity? 

Let's say I wanted to use a small amount of resin for example 5 KG in weight? How do I work out how much harder to use? 

I have made a mixture and it's been drying for 24 hours, however its still tacky, im assuming I have not used enough hardner? 
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
martynball - 9 Years Ago
oekmont - 9 Years Ago
Matt (Staff) - 9 Years Ago
Matt (Staff) - 9 Years Ago
martynball - 9 Years Ago
Matt (Staff) - 9 Years Ago
martynball - 9 Years Ago
GreyArea - 9 Years Ago
oekmont - 9 Years Ago
Warren (Staff) - 9 Years Ago
Capt Rouge - 9 Years Ago
Warren (Staff) - 9 Years Ago
Hanaldo - 9 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search