Hi Anders,
The oven comes packed with the electronics enclosure detached and inside the oven, so straight away you can take the enclosure and shelf separately to save some weight. You can also unbolt the front door assemblies. That might get it down to 60-65kg which should be possible to carry the oven with some help.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|