Hi Guys, 

I run and own an Automotive re-trim company, and I'd like to expand into carbon firber for interior parts. What I would really like to start up is covering parts of steering wheels in carbon fiber, and the rest trimmed in leather to offer my customers more options. Here is a picture of what I am talking about.. 

http://image.made-in-china.com/4f0j00LMnQuHTJAlbA/Auto-Carbon-Fiber-Steering-Wheel-Cover.jpg


How would I go about doing something like this? Would it be a similar process to the fishing rod repair?

Cheers
Steve
Reply
Warren
Warren
Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)
Group: Administrators
Posts: 214, Visits: 783
TBH youd beed to practice on a scrap wheel. Id think one layer is too thin as if driven aggressively there would be quite a big crush force on it.  Id start off with say 3 layers and if it feels super solid, then experiment with 2 layers.