Does your pump have a valve on it? I can't see from that photo. If there is no valve, then when you turn off the pump, air will try and go backwards through the pump reducing the vacuum level which could give you the effect you are seeing. otherwise you have a leak in the hose or around the hosetail barb fitting as the pump itself would unlikely cause a problem when it is running.