Group: Forum Members
Posts: 2,
Visits: 27
|
I think that I have a problem with my vacuum pump. The problem is that when I clamp the line between catch pot and my mold (drop test), the vacuum level change. But when I clamp the line between the pump and the catch pot, the vacuum level doesn't change . What's going on???
When I clamp the line like in the photo, the vacuum level doesn't change.
|