Hi guys using the twill 3k 200g cloth but is there any better to use for skinning?  Thicker but as easy to drape and shape to the parts? 
I find it can distort very easy.

Thanks
Reply
MarkMK
MarkMK
Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)
Group: Forum Members
Posts: 338, Visits: 2K
Hi

I'd highly recommend using the slightly more expensive 240g cloth that EC sells, as it is far more stable than the 200g equivalent and better suited to skinning jobs where a bit of drape is required