To me it looks like you are simply not making sure to get the corner areas of your layup wetted through enough When doing wet-lay I always wet out each layer one at a time using PLENTY of resin and a stiff brush . in wet-lay you can not calculate the amount of resin as 50-50 you will be lucky to get 55 resin and 45 fibre by weight ratio The breather cloth will get rid of most of the excess resin, but compared to infusion you will still have a more resin rich part