Hello friends, 
I made two pieces of carbon fiber by the hand lay up process + Vac bagging and I'm having problems with areas as per the picture. Defects such as air bubbles and dry regions.
I am not using Gel coat because I will use clear coat when finalizing and I do not use tacky spray because it is a cosmetic piece.

I'm using material / resin ratio in 50:50 and vacuum at -28 in.
Where can I be going wrong?

scottracing
scottracing
Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)
Group: Forum Members
Posts: 460, Visits: 5.2K
it also looks like a bit of bridging in the corners,you need to ensure that you prod the material with a suitable 'dibber' to force the material into the corner as the vacuum bag will not be enough to force the material into tight radius.