Yes, it would be fine to use the same adhesive film that you used for the aramid honeycomb with aluminium honeycomb. Make sure of course that the adhesive film has been stored frozen for the whole time since last year.
I hope this helps.
Matt Statham Easy Composites / Carbon Mods - Technical Sales
|