You will need to give the mould surface a good key with sand paper to ensure you get a bond, then lay on the resin and fibreglass thick enough this time so that it exotherms fully during the cure. This typically needs the 4 layers to achieve this.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|