Uni-mould question


Author
Message
flamypie
flamypie
Supreme Being (80 reputation)Supreme Being (80 reputation)Supreme Being (80 reputation)Supreme Being (80 reputation)Supreme Being (80 reputation)Supreme Being (80 reputation)Supreme Being (80 reputation)Supreme Being (80 reputation)Supreme Being (80 reputation)
Group: Forum Members
Posts: 9, Visits: 45
So i made the mistake of starting to lay the tooling resin without having enough resin to complete the 4 layers of 450grm CSM and only got 2 layers on,although quite resin rich. Is it ok to lay the second 2 layers days after or will i get some sort of de-lamination when using the tool at temperature? 
(i have learnt from my mistake)
thanks in advance.