Hi,
I like your ideas and will use them.

Will continue posting as I progress with my oven plans.

Thanks!
Tim
Tony2125
Tony2125
Supreme Being (211 reputation)Supreme Being (211 reputation)Supreme Being (211 reputation)Supreme Being (211 reputation)Supreme Being (211 reputation)Supreme Being (211 reputation)Supreme Being (211 reputation)Supreme Being (211 reputation)Supreme Being (211 reputation)
Group: Forum Members
Posts: 12, Visits: 59
Hi

I am building mine
I was wondering where should be the optimal position of the temperature sensor that control the PID.

Near the heating elements, to avoid overheating of any mold material.
Or inside the mold near the finish part to make sure the part cure at the set temperature 

Just let me know your thought, or feedback if ever experienced
Thanks
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search