Hi guys,

Just wondered if anyone has any tips on wetting out biaxial carbon fibre?

My first attempt was pretty poor using a paint brush, the material was so delicate it moved a lot of the fibres out of line and I ended up with some of it wavy rather than straight Ermm
scottracing
scottracing
Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)
Group: Forum Members
Posts: 460, Visits: 5.2K
get some of the different types of rollers on the market, you have bristled ones and the disc type, both should help you out