By Junior - 6/23/2017 12:15:56 PM
Hi guys,
Just wondered if anyone has any tips on wetting out biaxial carbon fibre?
My first attempt was pretty poor using a paint brush, the material was so delicate it moved a lot of the fibres out of line and I ended up with some of it wavy rather than straight
|
By scottracing - 6/23/2017 2:06:18 PM
get some of the different types of rollers on the market, you have bristled ones and the disc type, both should help you out
|
|