Leviatano55
Leviatano55
posted 8 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 3,
Visits: 51
I just bought my first sports car (Porsche Boxster) and I want to give it a touch of carbon fiber on the exterior. I am planning on buying two exposed carbon fiber mirrors. Would I be able to add two extra clear coats (one tinted) to give it a colored carbon look, or can I not paint carbon once it is fully finished?
thanks
Edited
8 Years Ago by
Leviatano55
Reply
Like
7
Reply
Leviatano55
Leviatano55
posted 8 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 3,
Visits: 51
Interloper393 (14/05/2017)
Candy paints are great over carbon pieces, then clear coat them
I agree, I think it vastly improves the look of carbon fiber.
Hanaldo (13/05/2017)
Absolutely, no problem.
Thanks!
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Can I color finished carbon fiber parts?
Leviatano55
-
8 Years Ago
Absolutely, no problem.
Hanaldo
-
8 Years Ago
Candy paints are great over carbon pieces, then clear coat them
Interloper393
-
8 Years Ago
[quote][b]Interloper393 (14/05/2017)[/b][hr]Candy paints are great over carbon pieces, then clear...
Leviatano55
-
8 Years Ago
I would be interested to see what a part looks like with a tinted clear coat on top.
polaraligned
-
8 Years Ago
[quote][b]polaraligned (15/05/2017)[/b][hr]I would be interested to see what a part looks like with...
Leviatano55
-
8 Years Ago
Post Reply
Like
7
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search